Introduction to the new process of forging and pulling length of large forgings

Home / News / Introduction to the new process of forging and pulling length of large forgings

Introduction to the new process of forging and pulling length of large forgings

In recent years, with the rapid rise of iron and steel, energy and petrochemical industries, forging into the process of forging production in the weight continues to increase, high dimensional accuracy requirements, the quality of ingots, which makes the entire forging work internal quality control has become more stringent, resulting in the traditional upsetting, pulling the length of the deformation of the forging process gradually can not be today's forging production requirements, for this reason it is necessary to take the work of new technologies to be carried out! Research and analysis, in order to ensure the smooth progress of forging work.
 First, large forgings forging process analysis
Large forgings are today's metallurgy, electric power, chemical industry, petroleum, transportation and other large-scale production of complete sets of facilities, the core components in the construction of the national economy and the development of modern society has a pivotal role. But today's large forgings forging and production process analysis, which is faced with the problem is still more prominent. For this reason, in today's large forgings forging production process, we need to analyze and summarize its forging process.

Second, large forgings forging process analysis
In the forging process of large forgings, in order to completely eliminate the defects that exist within the ingot, improve the quality of the structure, in the process of forging, in addition to choosing a reasonable supporting equipment, for the forging process and forging technology should also be given great importance and recognition.