| AISI/ASTM/ASME | 
EN | 
| A105 | 
1.0460  | 
| LF2 LF3 LF6 | 
1.0460  | 
| A694 F50 F52 F60 F65 F70 | 
/ | 
| F11 | 
1.7335 | 
| F12 | 
1.7335 | 
| F22 | 
1.7380  | 
| F5/F5a | 
1.7362 | 
| F9 | 
1.7386 | 
| 4130 4140 4145  | 
1.7218/ 1.7225 | 
| 4330/4330V 4340 | 
1.6582 | 
| 8620 8630  | 
1.6543/ 1.6545 | 
| F91 | 
1.4903 | 
| F92 | 
1.4922 | 
| 410/F6a | 
1.4006  | 
| 420 | 
1.4021 | 
| 431 | 
1.4057 | 
| F304 F304L F304H | 
1.4301/1.4306/1.4948 | 
| F316 F316L F316H F316LN F316Ti | 
1.4401/1.4404/1.4436/1.4571 | 
| F321 F321H | 
1.4541 | 
| F347 F347H | 
1.4551/1.4912 | 
| A182 F51 | 
1.4462 | 
| A182 F53 | 
1.4410  | 
| A182 F55 | 
/ | 
| A182 F60 | 
/ | 
| F6NM | 
1.4313 | 
| FXM-19 | 
/ | 
| 630 | 
1.4542 | 
| Nickel Alloy N04400 | 
 | 
| Nickel Alloy N05500 | 
 | 
| Nickel Alloy N06600 | 
 | 
| Nickel Alloy N06625 | 
 | 
| Nickel Alloy N07718 | 
 |