Destructive and Non-Destructive Testing
All our forgings are 100% UT as per ASTM, API or customer specified specifications. Chemistry validation is 100% per heat. Destructive testing is per heat lot to verify mechanicals meeting the requirements. Testing Chemistry ConfirmationHardness (Rockwell C and Brinell)Tensile TestingCharpy Impact testing (-150 degree C)Microstructure AnalysisUT (ASNT levell II)MPI (ASNT levell II)LPI (ASNT levell II)